Skip to article frontmatterSkip to article content
Site not loading correctly?

This may be due to an incorrect BASE_URL configuration. See the MyST Documentation for reference.

Found in the Polymer module, on the Ion conductivity tab.

Predicts the ionic conductivity of a polymer, in mS/cm, from its repeat unit, using molecular dynamics. Three kinds of system are covered:

Repeat unit chargeSystemMobile ions
positiveanion-exchange membrane (AEM)OH⁻, HCO₃⁻, Cl⁻, Br⁻, TFSI⁻ or FSI⁻, one per positive charge
negativecation-exchange membraneLi⁺, Na⁺ or K⁺, one per negative charge
neutralsalt dissolved in the polymer (polymer electrolyte, e.g. PEO + LiTFSI)the salt’s cation and anion

The charge is read from the SMILES, and the sidebar shows the ion choices that fit it.

This is a screening tool. It is designed to rank candidates against each other in roughly half an hour to an hour each, not to reproduce an absolute experimental conductivity.

Input

Repeat unit. Give the monomer as SMILES, or press 📂 Structure file and load any structure format the app reads (SDF/MOL, MOL2, PDB, XYZ, CDXML, QM inputs and outputs). Press ◎ Show & pick for a SMILES. The monomer appears in a viewer: click the two atoms where the chain continues. Clicking an atom replaces one of its hydrogens with the connection; clicking a hydrogen replaces that hydrogen. Click an atom again to undo it. For PEO, enter CCO and click the first carbon and the oxygen.

When the monomer has an aromatic ring, a suggested pair is already marked in green; click two atoms to choose others. The result appears in the Repeat unit field with * at the connections, e.g. *CCO*. You can also type a *-marked SMILES there directly.

A structure file must contain the repeat unit alone, with all its hydrogens and without counter-ions. Bonds are worked out from the geometry, so for a charged repeat unit set the net charge before loading the file.

The net charge per repeat unit is read from the SMILES and can be edited. Draw ionic groups in their ionised form: a sulfonate as S(=O)(=O)[O-], a quaternary ammonium as [N+](C)(C)C.

Ions.

SettingDefaultMeaning
Water uptake25 wt% for a charged polymer, 0 (dry) for a neutral onewater mass relative to the dry polymer
Chain length P10repeat units per chain
Number of chains3
Soaking solutionpure wateranion-exchange only: a salt of the mobile anion (e.g. NaOH, KCl) at a given molality
Temperature298.15 Kpolymer electrolytes are usually measured at 333–363 K
Equilibration21-step if dry, two-phase anneal (0.2 ns per phase) if hydratedsee below
Production2 ns for a hydrated membrane, 20 ns for a dry polymer electrolyteions in a dry polymer hop between slow polymer cages and need tens of ns to move diffusively
Replicas1more replicas give an error estimate
Ionic charge scaling (ECC)0.75electronic polarisation correction, applied to every ionic species
Applied electric field0 (off)after production, a second run with a uniform field along x; see Ion correlations below
Field run lengthsame as production
Vehicular fraction0.80OH⁻ only: the share carried by hydroxide diffusion, used to estimate the Grotthuss contribution

Force field and steps

Force fieldWhat it isSetup time
Standard (default)the app’s standard force field and charges; nothing is fitted to the monomerseconds
Refined for this monomerBoltzmann-weighted RESP charges and a refit of the sp²–sp² dihedrals against AIMNet2a QM job, minutes to an hour

With the standard force field, press ② Build & simulate directly: it sets the force field up itself. The refined one needs ① Parameterize monomer first. Either way the result depends only on the monomer, so it is cached and reused.

② Build & simulate tiles the repeat unit into chains, adds the ions and the water, equilibrates, and runs production MD. The conductivity follows from the ions’ diffusion via the Nernst–Einstein relation. Screening several chain lengths, water contents, ions or salt concentrations for the same monomer costs only this step each time.

Equilibration. A dry cell (no water, e.g. a polymer electrolyte) gets the 21-step compression/decompression protocol of Larsen et al. (2011): alternating stages at 600 K and at the target temperature, with the pressure raised to 50 kbar and released again, then 0.8 ns at the target conditions (1.56 ns in all). It is the standard way to bring an amorphous polymer to a reproducible density, and the log reports the density reached. A hydrated membrane keeps the shorter two-phase anneal, since taking water to 600 K and 50 kbar does nothing useful. Advanced → Equilibration protocol overrides the choice.

Ion parameters. Li⁺, Na⁺, K⁺, Cl⁻ and Br⁻ use the Joung–Cheatham parameters made for SPC/E water. OH⁻, HCO₃⁻, TFSI⁻ and FSI⁻ get their charges the same way as the polymer (standard, or RESP with the refined force field), once each, and are cached.

Ion correlations

The standard conductivity adds up each ion’s own diffusion as if it moved alone (Nernst–Einstein). Ions that move together, a cation and an anion as a pair or a cluster, carry no current but are counted there. Two other numbers measure the charge current itself:

Both use the formal ionic charges, like the standard number, so the three can be compared directly. If the collective or the field value is clearly lower than the standard one, ion pairs or clusters are reducing the conductivity.

Results